Insulation Material Phenolic Moulding Compound
Product Details:
Insulation Material Phenolic Moulding Compound Price And Quantity
- 10000 Piece
- 0.08 USD ($)/Piece
Insulation Material Phenolic Moulding Compound Trade Information
- Ningbo
- 50000000 Piece Per Month
- 10 Days
- Yes
- Contact us for information regarding our sample policy
- PAPER BOX, POLY BAG
- Western Europe Central America Middle East South America Asia Eastern Europe North America Australia Africa
- All India
Product Description
Insulation Material Phenolic Moulding Compound is precisely processed by our highly experienced experts utilizing the best grade chemical compounds and innovative processing technology. Offered array is extensively is used in production of insulation structures of low-voltage electric and electrical and appliance application. Our affording good electric characteristics and heat resistance; is suitable for compression molding. Provided Insulation Material Phenolic Moulding Compound is available in different packaging options as per the needs of our prestigious clients.
Technical Specifications
Unit | Standard | Indetexes |
|
Appearance | / | ZY/ZY .01-2015 | OK |
Density | g/cm3 | GB/T 1033. 1 | 1.79 |
Dsic Flow | Cm | ZY/ZY .01-2015 | 17 |
Flexural strength | MPA | GB/T 9341 | 220 |
impact strength(unnotchecd) | Kj/m2 | GB/T 1043.1 | 12 |
Volume resistivity | Ω.cm | GB/T 1410 | 1.0×1013 |
(Tf1.8Mpa) | oC | GB/T 1634.2 | 270 |
Moulding shrinkage | % | JB/T6542 | 0.1 |
Water absorption | % | GB/T 1034 | 0.1 |
Flame test UL-Subject 94 | UL94 | GB/5169. 16 | V-0 |
Electric strength | Kv/mm | GB/T 1408.1 | 14 |
Molding craft |
|
| compressing, transfer processing |
Compression Processing:
preheating temp. | preheating time | pressure | up mould temp. | down mould temp. | compression temp. | compression speed | pressure keeping time |
90-110ºC | 120-240S | 20-30MPA | 170oC | 160oC | 160-190oC | 5-20S | 120-240S |
After Curing:
150oC | 180oC | 210oC | 230oC |
2hours | 6hours | 8hours | 3 hours |